Bolt Grade Chart โ€” SAE, ASTM & ISO Grades, Strength Ratings and Head Markings

Start with the mark on the head. The identification tree below routes you to the right standard system before you read a strength table, because the same looking number can mean different things in SAE, ISO and ASTM documents.

Identification tree ยท tap a marking

ISO metric

8.8 / 10.9 / 12.9

Metric property class under ISO 898-1. The first number times 100 is minimum tensile strength in MPa; the second number times ten is the yield ratio as a percentage of tensile. Class 10.9 therefore promises at least 1000 MPa tensile and 900 MPa yield.

Bolt Grade Systems Overview

A bolt grade is a promise made by a standard. It tells the minimum strength the manufacturer must achieve in testing and, usually, how that promise is marked on the head. Three systems dominate the bolts you will meet: SAE J429 for imperial machine bolts, ISO 898-1 for metric property classes, and a family of ASTM product specifications for structural, stud and specialty fasteners.

The SAE system uses ordinal numbers: Grade 2, Grade 5 and Grade 8. Higher means stronger, and the exact tensile, yield and proof values come from J429 tables. The ISO system uses a two-part property class whose digits encode the numbers directly, which is why 8.8 can be decoded without opening the standard. ASTM specifications are product-based: A307 describes a low-carbon bolt, F3125 covers structural bolt grades, and A193 B7 describes an alloy-steel stud for elevated temperature.

These systems overlap in strength but not in requirements. A metric class 8.8 bolt and an SAE Grade 5 bolt sit in a similar strength band; a class 10.9 and Grade 8 sit in another. That does not make them interchangeable, because proof load, ductility, head geometry, nut matching and marking rules differ. The homepage of this site already gives the torque and preload implications of grade choice; this page concentrates on identification and the standard definitions behind the marks.

What this page does not repeat

The homepage grade section already publishes a strength chart, a preload target ladder and an answer to the strongest-grade question. Those conclusions are not duplicated here. This is an identification and standards reference, not a second copy of the same comparison.

SAE Bolt Grades Chart

Minimum tensile and yield strengths from the site's shared grade data, which follows SAE J429 for imperial grades. Values are converted from ksi at 6.894757 MPa per ksi and rounded to whole units.

GradeStandardTensile minYield minTypical head mark
SAE Grade 2SAE J42974 ksi / 510 MPa57 ksi / 393 MPaNone or two lines
SAE Grade 5 / ASTM A325SAE J429120 ksi / 827 MPa92 ksi / 634 MPaThree radial lines
SAE Grade 8SAE J429150 ksi / 1034 MPa130 ksi / 896 MPaSix radial lines

Grade 2 is the everyday low-strength hardware grade; Grade 5 is the general automotive and machinery workhorse; Grade 8 is the high-strength choice for heavy equipment. Head markings are the conventional radial-line patterns in SAE J429; confirm against the current standard and the manufacturer's certificate for safety-critical hardware.

Metric Bolt Property Classes Chart

ISO 898-1 property classes encode their own strength. The first number times 100 is the minimum ultimate tensile strength in MPa; the second number divided by ten is the ratio of yield to tensile. The table lists the resulting minimums for the most common classes.

ClassTensile minYield minHead markApplication band
Class 8.8800 MPa640 MPa8.8Metric structural workhorse
Class 10.91040 MPa940 MPa10.9Heavy equipment and high-strength joints
Class 12.91220 MPa1100 MPa12.9Maximum common commercial class

Lower metric classes exist for general hardware, and stainless property classes use a different designation scheme. Always read the full callout: the digits promise minimums by specification, not the measured strength of an individual bolt.

Structural grades

ASTM Structural Bolt Grades

Structural bolts are specified by product standard rather than by an SAE ordinal. The table shows how the familiar names relate to the current ASTM F3125/F3125M system and what each family is used for.

DesignationStandard familyStrength levelWhere it belongs
A307 Grade AASTM A30760 ksi minimum tensileLight structural and anchor work
A325 / F3125 Gr A325ASTM F3125/F3125M120 ksi (105 ksi over 1 in), historical A325 levelStructural steel bearing-type and slip-critical connections
A490 / F3125 Gr A490ASTM F3125/F3125M150 ksi classHigh-strength structural connections; no hot-dip galvanizing
A193 B7ASTM A193Alloy steel, quenched and temperedStuds for elevated temperature and pressure service
F1852 / F2280ASTM F3125/F3125MTwist-off assembly gradesTension control structural assemblies

A325 and A490 were separate historical ASTM specifications; F3125/F3125M consolidated the structural bolt grades under one document. Old drawings still use the former names. Verify the edition and grade callout in the project specification rather than assuming that every occurrence of a historic name carries identical current requirements.

Close-up of hex bolt heads with grade markings on a steel assemblyMarkings identify a grade, not a tested batchPhoto: Unsplash

Limit of visual identification

A marking tells you what a bolt is supposed to be. It cannot prove the batch passed testing, and an unmarked head is not a grade. Use certified hardware for critical connections.

Bolt Head Markings Identification

Markings fall into three visual families. Numeric property classes appear as two digits with a dot, defined by ISO 898-1. SAE grades use radial lines on the head, with three lines for Grade 5 and six for Grade 8 under J429. ASTM product grades are stamped as letters and numbers such as A307, A325, A490 or B7, sometimes with a manufacturer identifier alongside them.

Read the mark before reading a strength table. A bolt whose head shows six radial lines is in a different standard family from one stamped 10.9 even if their strengths are close. Symbol markings and manufacturer logos can sit next to the grade mark; the grade is the part defined by the standard, not the logo.

Grade / classTypical markingFamilyIdentification note
SAE Grade 2Typically unmarked, sometimes two radial linesLow-strength general hardwareVerify with certificate if unmarked
SAE Grade 5Three radial linesAutomotive and machinery general useStrength level near ISO class 8.8
SAE Grade 8Six radial linesHeavy equipment and critical imperial jointsCloser to ISO class 10.9
ISO 8.88.8 stamped on the headMetric structural workhorse800 MPa tensile, 640 MPa yield
ISO 10.910.9 stamped on the headHigh-strength metric assemblies1040 MPa tensile, 940 MPa yield
ISO 12.912.9 stamped on the headMaximum common commercial metric class1220 MPa tensile, 1100 MPa yield
ASTM A307A307 or maker mark; low strengthLight structural and anchor applications60 ksi minimum tensile for Grade A
ASTM F3125 A325A325 or F3125 Grade A325 markingStructural steel connections120/105 ksi historical strength level
ASTM F3125 A490A490 or F3125 Grade A490 markingHigh-strength structural connections150 ksi class; do not galvanize
ASTM A193 B7B7 marking on studsHigh-temperature and pressure serviceAlloy steel, quenched and tempered

Head stamps wear, corrode and can be obscured by paint. When the mark is incomplete, do not infer a grade from diameter, finish or application. Replace the fastener with traceable hardware or verify it through certificate records.

Strength Comparison and Approximate Equivalence

The useful comparison is by strength band, not by exact equality. Class 8.8 at 800 MPa tensile sits near SAE Grade 5 at 120 ksi (827 MPa). Class 10.9 at 1040 MPa sits near Grade 8 at 150 ksi (1034 MPa). A490 is also a 150 ksi class. These are minimum specification values in consistent units, not measured batch results.

Proof load is the comparison that matters most for tightening. It sits below yield and is the stress a bolt survives without measurable permanent stretch. Two bolts with similar tensile strength can carry different proof loads, which is why a cross-system substitution can change the clamp force a given torque produces. The homepage explains the 75 percent and 90 percent preload targets that build on proof and yield; this page stops at the grade definitions.

Grade 5 versus Grade 8

Grade 8 raises tensile from 120 ksi to 150 ksi and yield from 92 ksi to 130 ksi. The gain comes with reduced ductility, so Grade 8 is not automatically the safer choice in a joint that needs plastic redistribution.

8.8 versus 10.9

Class 10.9 lifts tensile from 800 MPa to 1040 MPa and yield from 640 MPa to 940 MPa. That extra preload capacity is useful in high-strength joints but leaves less margin against over-tightening and hydrogen-related issues.

Choosing the Correct Bolt Grade

Start with the design. The joint's load, connection type, environment and code determine the acceptable grade; the chart helps you recognise that grade once it arrives on site. Choosing the highest number on the shelf is not a design method. High-strength bolts are less ductile, more sensitive to coating restrictions and more demanding on matching nuts and washers.

Match the nut and washer to the bolt grade. A high-strength bolt in a low-strength tapped hole can strip the internal thread before the bolt reaches its own capacity, which is the failure mode the thread engagement calculator addresses. In structural work the bolt, nut and washer are specified as a system; substituting one component can void the connection's qualification.

Consider the service environment. Elevated temperature calls for grades designed for it, such as ASTM A193 B7 studs. Corrosive exposure may require a coating, and the coating must be compatible with the grade: A490-class fasteners must not be hot-dip galvanized. Fatigue-prone joints favour details that reduce stress concentration rather than simply a higher strength number.

Grade selection is not connection design. Once a grade is identified, use the bolt tension calculator or the shear calculator to check capacity. Neither replaces bearing, tear-out, fatigue or code checks.

Coatings and Strength Data Notes

Zinc plating and hot-dip galvanizing do not change the strength grade printed on a bolt. They change the friction at the threads and under the head, which changes the relationship between wrench torque and achieved preload. A dry torque value applied to a lubricated or plated bolt can overstress it, so a coating change should trigger a fresh look at the tightening specification.

Some coatings interact with high-strength grades in more serious ways. Hydrogen embrittlement is the reason ASTM A490 fasteners must not be hot-dip galvanized. Always check the standard and the manufacturer's data sheet for the specific grade and coating pair before specifying it.

The numbers in this chart are minimums from the specifications, not typical test values. A real batch of class 8.8 bolts often measures above 800 MPa, but designing against the typical value would quietly remove the safety margin the grade mark promises. Units are stated throughout: MPa for metric strength and ksi for imperial strength, converted at 6.894757 MPa per ksi.

Do not place proof load, yield strength, tensile strength and code design strength in one column. They come from different tests and different resistance factors, and mixing them is the fastest way to reach a wrong conclusion.

Identify, Then Calculate

This bolt grade chart is the upstream reference for the site's calculators. Once the mark is decoded, the bolt torque spec chart gives starting torque values and the thread pitch and stress area chart gives the area each strength check uses. The homepage applies grades to preload targets, and the full library sits on the guides hub.

FAQ

Bolt Grade Chart FAQ

Markings, standards, strength definitions and cross-system comparisons.

What is a bolt grade chart?
A bolt grade chart maps the markings on a bolt head to the strength promised by a standard. It connects systems that use different naming rules: SAE J429 numeric grades for imperial bolts, ISO 898-1 property classes for metric bolts, and ASTM product specifications such as A307, F3125 A325/A490 and A193 B7. A useful chart states the standard, the marking, and the minimum tensile and yield strengths in consistent units.
How do I identify a bolt grade from head markings?
Start with the shape of the mark. Two numbers separated by a dot indicate a metric ISO property class. Three radial lines on an imperial hex head indicate SAE Grade 5, and six indicate Grade 8. Letter designations such as A325, A490 or B7 point to ASTM product grades. An unmarked head is not evidence of a low grade: it may be non-standard, worn or counterfeit. For critical joints, rely on traceable certification rather than appearance alone.
What does 8.8 mean on a bolt?
It is an ISO 898-1 property class. The first digit times 100 gives the minimum ultimate tensile strength in megapascals, so 8 means 800 MPa. The number after the dot is the yield ratio: 0.8 times 800 gives a minimum yield of 640 MPa. Class 10.9 works the same way, with 1000 MPa tensile and 900 MPa yield. The rule describes minimum values by specification, not the actual test result of a particular batch.
What is the difference between Grade 5 and Grade 8 bolts?
Both are SAE J429 imperial grades. Grade 5 has a specified minimum tensile strength of 120 ksi and yield near 92 ksi; Grade 8 raises those to about 150 ksi tensile and 130 ksi yield. Grade 5 carries three radial head lines, Grade 8 carries six. Grade 8 is stronger but less ductile, so it is not automatically the better choice; the joint design, nut grade and loading mode decide.
Are metric 8.8 and SAE Grade 5 the same?
They are close in minimum tensile strength, which is why they are often treated as rough neighbours in non-critical work, but they are defined by different standards with different proof loads, ductility requirements and head markings. Substituting one for the other without checking the governing specification can change the preload a joint delivers. Treat cross-system comparisons as orientation, not as a substitution licence.
What is the difference between A325, A490 and ASTM F3125?
A325 and A490 were separate ASTM specifications for structural bolts at 120/105 ksi and 150 ksi strength levels. ASTM F3125/F3125M consolidated those and related head markings into a single specification with grades such as F3125 Grade A325 and F3125 Grade A490. Older drawings still say A325 or A490; newer ones may use the F3125 designation. They refer to comparable structural bolt families, but the current standard text governs requirements.
What is proof load and why is it different from tensile strength?
Proof load is the maximum stress a bolt withstands in a test without measurable permanent deformation, usually measured at a small offset. Tensile strength is the stress at rupture, and yield is where permanent stretch begins. Proof sits below yield and well below ultimate. Preload targets are conventionally set against proof so a reusable bolt springs back to its original length after tightening; ultimate strength is the overload margin.
What does ASTM A307 cover?
ASTM A307 is a specification for low-carbon steel bolts, studs and threaded rods. Grade A has a minimum tensile strength of 60 ksi and is common in light structural work, anchors and general fastening where high strength is not required. It is not a substitute for A325 or A490 structural grades. Its head markings are minimal, which is one reason an unmarked bolt should never be assumed to be a high grade.
Do coatings change a bolt's grade?
No. Zinc plating or hot-dip galvanizing does not change the strength grade defined by the standard, but the coating changes friction, which changes the relationship between applied torque and achieved preload. Some high-strength grades have coating restrictions: ASTM A490 fasteners must not be hot-dip galvanized because of hydrogen embrittlement risk. Always follow the standard and manufacturer guidance for the grade and coating combination.
Can I choose a bolt grade by strength alone?
No. Strength is one input. The connection also needs compatible nuts and washers, adequate ductility, resistance to hydrogen embrittlement, appropriate behaviour under fatigue, and compliance with the governing code. A higher grade can be more brittle and less forgiving of over-torque. Use this chart to identify and understand a grade, then let the joint design determine which grade is acceptable.

Sources and scope. Strength values follow ISO 898-1 for metric property classes, SAE J429 for imperial grades and ASTM A307 / F3125 / A193 product specifications, as implemented in the site's shared bolt data. Head-marking patterns are conventional descriptions from those standards; confirm against the current edition and manufacturer certification for critical hardware. ksi to MPa uses 6.894757 MPa per ksi.

Author & update. Bolt Calculatorengineering content team ยท Last updated 2026-11-23 ยท Data current to 2026-11-23. This chart is a reference for identification; it does not certify a bolt or replace a connection design reviewed by a qualified engineer.